Home/News/Drawing Triangular Wire: Carbide Dies, Ceramic Dies and Why the Die Makes the Corner
Drawing Triangular Wire: Carbide Dies, Ceramic Dies and Why the Die Makes the Corner
Corner quality on triangular wire is decided in the die, not at inspection. Where tungsten carbide earns its keep, where ceramic (and NiB-coated) dies pay off, and how die wear shows up as slot drift on the finished screen.
Ask a screen maker why one supplier's triangular wire winds better than another's at the same nominal size, and the honest answer is usually one word: dies. The triangle's corner radii, face flatness and dimensional drift over a coil are all decided at the die face, a few tenths of a millimetre of tungsten carbide doing work that inspection can only sort, not fix. This page is the plain version of what we do at that stage.
The pass schedule, briefly
A triangular profile is not drawn to shape in one pass. The round or square feed bar is reduced through a sequence of shaped passes — typically a nested set of profiled carbide blocks held in a steel casing — with each pass removing area and moving material toward final geometry. Getting the corner radius right means leaving enough strain in the final passes to sharpen the corners while not over-working the wire; too aggressive a finish and the corners chip dies or the wire springs, too gentle and the triangle stays soft-edged and the finished slot reads smaller than the pitch says.
Tungsten carbide: the workhorse
Profile dies are almost always tungsten carbide — hard enough to hold a corner geometry for hundreds of kilometres of wire, tough enough to survive the side loads a shaped pass generates. Carbide's failure mode is gradual wear at the bearing surface, which shows up slowly as a profile that gets very slightly larger and rounder-cornered along a production run. That drift is why we sample-check geometry at coil start, mid and end — not once per batch.
Where ceramic (and NiB-coated) dies pay off
Ceramic dies — and nickel-boron coated steels in lighter duty — earn their keep on surface finish and lubricity: lower friction at the bearing means less die wear per tonne and a brighter, more uniform wire face, which matters when that face becomes the screening surface of a wedge wire screen. The trade-offs are real: ceramic is more brittle under shock and side load, and the tooling costs more upfront. For fine profiles where the wrap face carries the tolerance — and for stainless grades where galling is a risk — the payoff is measured in fewer off-spec metres and better slot consistency on the customer's winding machine. For coarse profiles on short runs, carbide usually wins the economics.
What die wear looks like downstream
The end user never sees a worn die — they see its signature. Slot scatter on a finished screen (a screen built at constant pitch holding different actual slots along the wrap) traces back to profile drift along a coil, which traces back to die wear that was never resampled. This is why our screen-wrap wire is specified with the wrap face at h9–h11 and checked at coil start, mid and end: the checks exist to catch the die, not the wire.
Questions worth asking any shaped-wire supplier
- How is corner radius held, and at which pass is it fixed?
- What is the die material per profile size, and why?
- How often is geometry re-sampled within a coil — and can you see the records?
- What happens between passes to keep the surface clean enough for the next die?
The wire this feeds is on the triangular wire list, the general manufacturing flow (melting to straightening) is on the process page, and what the tolerances mean to a buyer is in the tolerance guide. Send the profile and the duty — if the corner geometry is the deciding factor for your screen, the quote will say so plainly instead of hiding it in a tolerance band.
More from ERQI
-
Technical
Keeping a Wedge Wire Screen Clean: Backwash, CIP and Telling Fouling from Wear
Most wedge wire problems are fouling, not wear. Match the cleaning to the deposit, build backwash in from the first drawing, and measure slot instead of guessing - the difference shows in the delta-P trend.
-
Technical
Wedge Wire Screens or Perforated Plate: Choosing the Opening
Perforated plate is cheaper, stronger in the flat and available in any workshop; wedge wire has three times the open area and clears itself. The decision usually turns on open area, blinding and where the wear lands.
-
Technical
How to Specify a Wedge Wire Screen: The Five Numbers That Matter
A wedge wire screen quotation is a five-number conversation: slot width, wire profile, support rod, open area and material. What each number decides, how they trade against each other, and what a complete RFQ looks like.
Ready to start your project?
Send us your drawing or sample — we reply within 24 hours on working days.